View the report above. Use the comments below if you need follow-up discussion.
Material direction: Copolymerized polypropylene
The FTIR spectrum is dominated by strong aliphatic C–H stretching and bending absorptions consistent with a polypropylene‑based material. The reference library comparison returns Copolymerized PP as the top match (similarity 0.875), and the fifteen leading candidates are all polypropylene or PP‑copolymer formulations, confirming the polyolefin backbone FTIR In-Depth Interpretation was not selected for this task, so this section shows the library-search result only and no deep AI interpretation was run.
| Rank | Match % | Compound | Formula / SMILES | Library Preview | Action |
|---|---|---|---|---|---|
| Loading library candidates... | |||||
| # | Wavenumber (cm⁻¹) | Absorbance | Assignment | Citation | Confidence | |
|---|---|---|---|---|---|---|
| 1 | · | 2917 | 1.00 | - | - | - |
| 2 | · | 1375 | 0.59 | - | - | - |
| 3 | · | 2950 | 0.55 | - | - | - |
| 4 | · | 1458 | 0.42 | - | - | - |
| 5 | · | 2847 | 0.39 | - | - | - |
| 6 | · | 2868 | 0.33 | - | - | - |
| 7 | · | 1000 | 0.18 | - | - | - |
| 8 | · | 1033 | 0.17 | - | - | - |
| 9 | · | 467 | 0.13 | - | - | - |
| 10 | · | 1359 | 0.13 | - | - | - |
| 11 | · | 973 | 0.13 | - | - | - |
| 12 | · | 1101 | 0.13 | - | - | - |
| 13 | · | 719 | 0.11 | - | - | - |
| 14 | · | 1166 | 0.10 | - | - | - |
| 15 | · | 841 | 0.09 | - | - | - |
| 16 | · | 537 | 0.09 | - | - | - |
| 17 | · | 424 | 0.07 | - | - | - |
| 18 | · | 3695 | 0.06 | - | - | - |
| 19 | · | 809 | 0.06 | - | - | - |
| 20 | · | 900 | 0.06 | - | - | - |
| 21 | · | 1633 | 0.05 | - | - | - |
| 22 | · | 2722 | 0.04 | - | - | - |
| 23 | · | 3155 | 0.04 | - | - | - |
| 24 | · | 876 | 0.03 | - | - | - |
Use this area to continue the interpretation, ask questions, or add extra verification evidence.